Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 688 - 788 °C
1270 - 1450 °F
Brazing Range
Lucas-Milhaupt FOS FLO 670 Copper Phosphorus Tin Braze Filler Metal
Applications:Fos-Flo 7 iFos-Flo 670 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encounter..
Processing Temperature 707.2 - 788 °C
1305 - 1450 °F
Brazing Range
Lucas-Milhaupt Premabraze 616 Silver Based Cadmium Free Filler Metal
Applications: Application is found in all types of moderate temperature low pressure systems, and in particular the electronic vacuum tube. Characteristics:Premabraze 616 is a low temperature, sl..
Processing Temperature 690.6 - 788 °C
1275 - 1450 °F
Brazing Range
Lucas-Milhaupt SIL-FOS 6 Silver/ Copper/ Phosphorus Alloy
Applications: Sil-Fos 6 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in servi..
Processing Temperature 704 - 788 °C
1300 - 1450 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® 2 Brazing Alloy
Silvaloy 2 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on ..