Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 130 - 170 °C | 266 - 338 °F | Sheet Forming |
Polycasa PS QUINN PS sheets have good optical properties and a brilliant surface. The QUINN PS range contains sheets that are easy to fabricate, to vacuum form, and show a high light transmission (min 88% wavel.. |
|||
Processing Temperature | 160 - 170 °C | 320 - 338 °F | Mixture Zone |
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength.. |
|||
Processing Temperature | 160 - 170 °C | 320 - 338 °F | Plasticizing Zone |
Petroquimica Triunfo Trithene® TS 9022 MDPE - Overwrap Packaging The Trithene TS 9022 resin is a medium-density polyethylene (MDPE) with good optical properties, excellent stiffness and processability, that warrants the production of thin films with good appearan.. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® AFR/720 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Processing Temperature | 155 - 170 °C | 311 - 338 °F | Plasticizing Zone |
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing .. |
|||
Processing Temperature | 155 - 170 °C | 311 - 338 °F | Mixture Zone |
Petroquimica Triunfo Tritheva® TN 2007 EVA Copolymer The Tritheva TN 2007 resin is an Ethylene-Vinyl Acetate copolymer (EVA), developed to meet the multi-layer packaging needs where are required high strength, with high toughness, and excellent optica.. |
|||
Processing Temperature | 155 - 170 °C | 311 - 338 °F | Mixture Zone |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
Processing Temperature | 160 - 170 °C | 320 - 338 °F | Metering Temperature, Extrusion |
Stellarchem SV-B40D TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Processing Temperature | 160 - 170 °C | 320 - 338 °F | Metering Temperature, Extrusion |
Stellarchem SV-B65E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Processing Temperature | 160 - 170 °C | 320 - 338 °F | Metering Temperature, Extrusion |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Processing Temperature | 160 - 170 °C | 320 - 338 °F | Metering Temperature, Extrusion |
Stellarchem SV-B75E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Processing Temperature | 160 - 170 °C | 320 - 338 °F | Metering Temperature, Extrusion |
Stellarchem SV-B80E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Processing Temperature | 160 - 170 °C | 320 - 338 °F | Metering Temperature, Extrusion |
Stellarchem SV-B87E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Processing Temperature | 140 - 170 °C | 284 - 338 °F | |
Total EVA 1040 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1040 VN 4 is made by a high pressure tubular process. Grade for very flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Thin st.. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | |
Wanhua Chemical Wanthane® WHT-1680AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 140 - 170 °C | 284 - 338 °F | Glue Line Temperature |
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 140 - 170 °C | 284 - 338 °F | Lamination Adhesive |
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 140 - 170 °C | 284 - 338 °F | Lamination Adhesive |
EMS-Griltech Griltex® D 1439E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 140 - 170 °C | 284 - 338 °F | Films Die Head |
EMS-Griltech Griltex® D 1441E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 140 - 170 °C | 284 - 338 °F | Lamination Adhesive |
EMS-Griltech Griltex® D 1519E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 140 - 170 °C | 284 - 338 °F | Lamination Adhesive |
EMS-Griltech Griltex® D 1556A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 140 - 170 °C | 284 - 338 °F | Lamination Adhesive |
EMS-Griltech Griltex® D 1619E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | optimum shaping temperature |
Lucite International SW Sanitary Ware Acrylic Sheet Lucite® SW complies with ISO 7823-1 and EN 263. It is approved by the French ARNOR "NF" quality mark.Information provided by Lucite International |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | |
Taiwan Sheen Soon Sheenthane® A9612K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |