Polymer Property : Processing Temperature = 221 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 130 - 221 °C
266 - 430 °F
Average value: 188 °C Grade Count:17
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Processing Temperature 193 - 221 °C
379 - 430 °F
Blow Molding
Chevron Phillips Marlex® C579 High density polyethylene  (discontinued **)
Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceApplications: multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containersInformation pro..
Processing Temperature 193 - 221 °C
379 - 430 °F
Blow Molding
Chevron Phillips Marlex® C513 High density polyethylene  (discontinued **)
Benefits: outstanding impact and creep resistance, outstanding ESCR, excellent processabilityApplications: intermediate bulk containers, agricultural containersInformation provided by Chevron Philli..
Processing Temperature 204 - 221 °C
399 - 430 °F
Chevron Phillips mPact™ D449 HDPE Blown Film Resin  (discontinued **)
Resin Type: High density, hexene copolymerCharacteristics: excellent clarity, high gloss, good modulus, process with LLDPE setup, optimum clarity when used as an individual layer.Applications: overw..
Processing Temperature 193 - 221 °C
379 - 430 °F
Extrusion
Shuman 210 Polyphenylene Ether Copolymer Alloy
Black, Custom Colors. Good impact strength, easy processability, good chemical resistance, injection molding and extrusion grades.Data provided by the manufacturer.
Processing Temperature 193 - 221 °C
379 - 430 °F
Extrusion
Shuman 211 Flame Retardant Polyphenylene Ether Copolymer Alloy
Black, Custom Colors. Excellent flame retardancy, easy processability, good impact strength, good chemical resistance, injection molding and extrusion grades.Data provided by the manufacturer.
Processing Temperature 194 - 221 °C
381 - 430 °F
Optimum Extrusion Conditions
DSM Biomedical Elasthane™ 75D Thermoplastic Polyether Polyurethane (TPU)
A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility Elasthane™ TPU exhibits outstanding hydrolytic stabilit..
Processing Temperature 204 - 221 °C
399 - 430 °F
Optimum Extrusion Temperature
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer  (discontinued **)
Description: PELLETHANE® 2103-75D UV stabilized, polyether based thermoplastic polyurethane elastomer has excellent hydrolytic stability and excellent resistance to micro-organisms. Applications in..