Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shuman 210 Polyphenylene Ether Copolymer Alloy

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Molded
Manufacturer Shuman
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shuman 210 Polyphenylene Ether Copolymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Black, Custom Colors. Good impact strength, easy processability, good chemical resistance, injection molding and extrusion grades.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Melt Flow 1.3 g/10 min
1.3 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
ASTM D638
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
219 °F
ASTM D648
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 193 - 221 °C
379 - 430 °F
Extrusion
221 - 260 °C
430 - 500 °F
Injection
Users viewing this material also viewed the following: