BASF Elastollan B 95 A TPUR

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer BASF
Trade Name Elastollan
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan B 95 A TPUR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and superior low temperature flexibility.Typical Applications: Sport-shoe soles and accessories, ski-boot shells, technical moldings, e.g. seals, castor tyres and tubing.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
ISO 868
Hardness, Shore D 48
48
ISO 686
Tensile Strength 40.0 MPa
5800 psi
after storage in water at 80°C for 42 days; ISO 37
55.0 MPa
7980 psi
ISO 37
7.00 MPa

@Strain 20.0 %
1020 psi

@Strain 20.0 %
ISO 37
10.0 MPa

@Strain 100 %
1450 psi

@Strain 100 %
ISO 37
22.0 MPa

@Strain 300 %
3190 psi

@Strain 300 %
ISO 37
Elongation at Break 500 %
500 %
after storage in water at 80°C for 42 days; ISO 37
550 %
550 %
ISO 37
Charpy Impact, Notched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
DIN EN ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN EN ISO 179
Tear Strength 100 kN/m
571 pli
DIN ISO 34-1/Bb
Abrasion 30
30
[mm<sup>3</sup>; ISO 4649
Compression Set 30 %

@Temperature 23.0 °C
30 %

@Temperature 73.4 °F
ISO 815
40 %

@Temperature 70.0 °C
40 %

@Temperature 158 °F
ISO 815
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Injection molding
175 - 230 °C
347 - 446 °F
Extrusion
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Injection molding and Extrusion