Polymer Property : Processing Temperature = 385 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 385 °C
725 °F
Plasma Coatings 200-2 Surface Material
Information provided by Plasma Coatings
Processing Temperature 385 - 410 °C
725 - 770 °F
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:..