Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 385 °C | 725 °F | |
Plasma Coatings 200-2 Surface Material Information provided by Plasma Coatings |
|||
Processing Temperature | 385 - 410 °C | 725 - 770 °F | |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |