Polymer Property : Processing Temperature = 420 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 177 - 216 °C
350 - 420 °F
Extrusion
Shuman 710H Utility Black ABS
Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc.
Processing Temperature 177 - 216 °C
350 - 420 °F
Extrusion
Shuman 720H Black ABS
Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc.
Processing Temperature 177 - 216 °C
350 - 420 °F
Extrusion
Shuman 730 Utility White ABS
Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the Shuman Plastics, Inc.
Processing Temperature 177 - 216 °C
350 - 420 °F
Extrusion
Shuman 730H White ABS
Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc.
Processing Temperature 177 - 216 °C
350 - 420 °F
Extrusion
Shuman 780H Grey ABS
Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc.