Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 550 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 271 - 288 °C
520 - 550 °F
Oxford Polymers Oxnilon 6-33GF 33% Glass Fiber Filled Nylon 6 for Injection Molding
33% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
Processing Temperature 271 - 288 °C
520 - 550 °F
Oxford Polymers Oxnilon 6-43GF 43% Glass Fiber Filled Nylon 6 for Injection Molding
43% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
Processing Temperature 271 - 288 °C
520 - 550 °F
Oxford Polymers Oxnilon 6-50GF 50% Glass Fiber Filled Nylon 6 for Injection Molding
50% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
Processing Temperature 249 - 288 °C
480 - 550 °F
Profile Temperature
NOVA Chemicals Dylark® 238P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Processing Temperature 249 - 288 °C
480 - 550 °F
Profile temperatures
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
Processing Temperature 249 - 288 °C
480 - 550 °F
Profile temperatures
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin
Features: Ultra high modulus, High heat resistance, excellent adhesion to urethaneApplications: Instrument panel substrates, Brackets, Structural components
Processing Temperature 249 - 288 °C
480 - 550 °F
Profile Temperature
NOVA Chemicals Dylark® 480P12 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Processing Temperature 249 - 288 °C
480 - 550 °F
Profile temperatures
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin
Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati..
Processing Temperature 249 - 288 °C
480 - 550 °F
Profile Temperature
NOVA Chemicals Dylark® 250P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Processing Temperature 249 - 288 °C
480 - 550 °F
Profile temperatures
NOVA Chemicals Dylark® 378P12 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
Processing Temperature 249 - 288 °C
480 - 550 °F
Profile Temperature
NOVA Chemicals Dylark® 378P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Processing Temperature 249 - 288 °C
480 - 550 °F
Profile Temperature
NOVA Chemicals Dylark® 480P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Processing Temperature 266 - 288 °C
510 - 550 °F
Average value: 277 °C Grade Count:3
Overview of materials for Polycarbonate, Foam Grade, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum ..
Processing Temperature 227 - 288 °C
440 - 550 °F
Average value: 261 °C Grade Count:5
Overview of materials for Glass Reinforced, Modified SMA
This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of..
Processing Temperature 221 - 288 °C
430 - 550 °F
Soldering Range
Lucas-Milhaupt Silvabrite® S™ Lead-Free Solder
Silvabrite silver/tin soldering alloys have been engineered specifically for field repair. These silver/tin solders have been specifically formulated to make difficult repairs swiftly and confidentl..
Processing Temperature 266 - 288 °C
510 - 550 °F
Shuman 900 Clear Polycarbonate
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Processing Temperature 266 - 288 °C
510 - 550 °F
Shuman 910 Utility Black Polycarbonate
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Processing Temperature 266 - 288 °C
510 - 550 °F
Shuman 910-05V0 Utility Black Polycarbonate Glass Filled
Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc.
Processing Temperature 266 - 288 °C
510 - 550 °F
Shuman 920 Black Polycarbonate
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Processing Temperature 266 - 288 °C
510 - 550 °F
Shuman 930 White Polycarbonate
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Processing Temperature 266 - 288 °C
510 - 550 °F
Shuman 930-05V0 White Polycarbonate Glass Filled
Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc.
Processing Temperature 266 - 288 °C
510 - 550 °F
Shuman 980 Grey Polycarbonate
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Processing Temperature 266 - 288 °C
510 - 550 °F
Shuman 980-05V0 Grey Polycarbonate Glass Filled
Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc.
Processing Temperature 266 - 288 °C
510 - 550 °F
Shuman FR910V0 Utility Black Polycarbonate Flame Retardant
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Processing Temperature 266 - 288 °C
510 - 550 °F
Shuman FR980V0 Grey Polycarbonate Flame Retardant
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Copyright © lookpolymers.com All Rights Reserved