Processing Properties Metric English Comments
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® 3385A Polyurethane
Extrusion- and injection molding gradegood wear resistanceshort cycle timeshigh melt stabilityApplicationhard - soft systemsHosesnon-reinforcedProfilesInjection molded engineering partsPreprocessing..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® 481 Polyurethane
injection molding gradefree from plasticizersgrease and oil-resistantlow compression sethigh elasticitygood heat resistanceEasy releaseApplicationRoller coatingSealsmembranesAutomotive engineeringPr..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® 790 Polyurethane
Extrusion- and injection molding gradehigh mechanical strengthApplicationToothed beltsProfilesInjection molded engineering partsPreprocessingMax. Water content
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® 9385 Polyurethane
Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilitycomplies with VDE 0282-10ApplicationCable sheathingsHosesnon-reinforcedPreprocessin..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 1080A Polyurethane
injection molding gradefree from plasticizershard - soft systemsTechnical partsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covest..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 1485A Polyurethane
Extrusion- and injection molding gradesuitable for extrusion blow moldingvery large processing windowhigh melt stabilityBeadsApplicationBellowsHosesnon-reinforcedProfilesInjection molded engineering..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 2586A Polyurethane
Extrusion- and injection molding gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentBeadsApplicationBlown filmsPreprocessingMax. Water co..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 2590A Polyurethane
Extrusion- and injection molding gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationBlown filmsPreprocessingMax. Water content..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 2786A Polyurethane
Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 2792A Polyurethane
Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 3491A Polyurethane
Extrusion- and injection molding gradesuitable for extrusion blow moldinghigh mechanical strengthhigh melt stabilityApplicationBlow moldingProfilesInjection molded engineering partsPreprocessingMax...
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 3660DU Polyurethane
Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 3690AU Polyurethane
Extrusion- and injection molding gradehydrolysis-stabilisedwith special UV stabilizerswith release agenttransparent up to 6 mm wall thicknessgood wear resistanceApplicationSports shoe solesFilmsHose..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 3695AU Polyurethane
Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 5080A Polyurethane
injection molding gradeimproved microbial resistanceImproved hydrolysis resistanceApplicationSealsmembraneshard - soft systemsPreprocessingMax. Water content
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 6065A Polyurethane
injection molding gradefree from plasticizersvery good hydrolysis and microbial resistancevery short cycle timesApplicationhard - soft systemsShoe solesPreprocessingMax. Water content
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 8798A Polyurethane
injection molding gradewith special UV stabilizersEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 9095AU Polyurethane
injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood wear resistancelow warpargeshort cycle timesApplicationEar-tagsPreprocessingMax. Water content
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 9370A Polyurethane
Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission rateApplicationbreathable fi..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 9380A Polyurethane
Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilitycomplies with VDE 0282-10ApplicationCable sheathingsHosesnon-reinforcedPreprocessin..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 9392AU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityApplicationHosesnon-reinforcedCable sheathingsProfilesTe..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 9395AU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityApplicationPneumatic hosesProfilesCable sheathingsInject..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 9650DU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedAs of ..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 9659DU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 9662DU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® DP 9665DU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPneuma..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® W DP 85085A Polyurethane
injection molding gradeno yellowing under the action of UV lightimproved microbial resistancegood low-temperature flexibilityImproved hydrolysis resistanceApplicationautomotive interior applications..
Ejection Temperature 50.0 °C
122 °F
Covestro Desmopan® W DP 89051D Polyurethane
PreprocessingMax. Water content