Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Desmopan® DP 9095AU Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 9095AU Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood wear resistancelow warpargeshort cycle timesApplicationEar-tagsPreprocessingMax. Water content
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
Melt
1.15 g/cc
0.0415 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
3s; ISO 868
Hardness, Shore D 43
43
15s; ISO 868
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527-1/-2
Tensile Strength, Yield 50.0 MPa
7250 psi
parallel; ISO 527-3
16.0 MPa

@Strain 100 %
2320 psi

@Strain 100 %
ISO 527-1/-2
33.0 MPa

@Strain 300 %
4790 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 18
18
mm³; ISO 4649
Compression Set 30 %

@Temperature 23.0 °C
30 %

@Temperature 73.4 °F
ISO 815
77 %

@Temperature 70.0 °C
77 %

@Temperature 158 °F
ISO 815
Thermal Properties Metric English Comments
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Thermal Conductivity 0.132 W/m-K
0.916 BTU-in/hr-ft²-°F
Melt
Processing Properties Metric English Comments
Melt Temperature 200 - 220 °C
392 - 428 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Ejection Temperature 50.0 °C
122 °F
Descriptive Properties Value Comments
Availability Europe
Near East/Africa
South and Central America
Eff. thermal diffusivity (m²/s) 8E-08