Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 103 - 138 MPa | 15000 - 20000 psi | Average value: 121 MPa Grade Count:5 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Injection Pressure | 103 - 138 MPa | 14900 - 20000 psi | |
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | Average value: 88.7 MPa Grade Count:3 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | Average value: 89.1 MPa Grade Count:3 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | Average value: 95.2 MPa Grade Count:7 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | |
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | |
MRC Polymers MAXTELâ„¢ 600 GF20 TPO, 20% Glass Fiber Filled For automotive exterior applications. Excellent process ability and dimensional stability.Internal and external lubricants can be addedCan be UV StabilizedInformation provided by MRC Polymers Inc. |
|||
Injection Pressure | 69.0 - 138 MPa | 10000 - 20000 psi | |
Lavergne VYTEEN PC 135 General Purpose Medium Viscosity Polycarbonate Vyteen PC 135, Black, medium viscosity polycarbonate, has an excellent balance of stiffness and impact resistanceFeatures: - High heat resistance - Good processabilityInformation provided by Biegl.. |
|||
Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | |
MRC Polymers NAXELLâ„¢ PC23MS Polycarbonate, Impact Modified, High MFR, EZ Flow Economy GradeImpact modifiedCan be UV stabilizedGenerally for black onlyInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Injection Pressure | 110 - 138 MPa | 16000 - 20000 psi | |
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® 22LHI6 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® FR22F-N Flame Retardant Nylon 66, Lubricated Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® MR409 22H-N 40% Mineral Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® NY1599-N Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66 Description: Medium Impact Nylon 66Information provided by Wellman. |
|||
Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | |
Lubrizol Estane® 58144 Thermoplastic Polyurethane Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound.Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer.. |
|||
Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | Initial |
Clariant Renol PCSP0009 Polycarbonate, 15% Glass Fiber, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 138 MPa | 720 - 20000 psi | Average value: 43.2 MPa Grade Count:3 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Injection Pressure | 8.27 - 138 MPa | 1200 - 20000 psi | Average value: 34.8 MPa Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |