Processing Properties Metric English Comments
Injection Pressure 4.96 - 7000 MPa
720 - 1.02e+6 psi
Average value: 854 MPa Grade Count:4
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Injection Pressure 3000 - 7000 MPa
435000 - 1.02e+6 psi
Injection
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane
Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo..