Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 4.96 - 7000 MPa | 720 - 1.02e+6 psi | Average value: 854 MPa Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Injection Pressure | 3000 - 7000 MPa | 435000 - 1.02e+6 psi | Injection |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |