Processing Properties Metric English Comments
Injection Pressure 10.0 - 14.0 MPa
1450 - 2030 psi
M. Holland Company MAGMA® Magmalene Polyalphaolefin  (discontinued **)
High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessUses: BlendingProcessing Method: Injection MoldingInformation provided by M. Holland.
Injection Pressure 10.0 - 14.0 MPa
1450 - 2030 psi
M. Holland Company MAGMA® LM372-A LLDPE  (discontinued **)
Features: High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessProcessing Method: Injection MoldingInformation provided by M. Holland.
Injection Pressure >= 10.0 MPa
>= 1450 psi
Compression and injection cavity mold pressure
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage  (dis
Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l..
Injection Pressure 10.0 MPa
1450 psi
Lubrizol Advanced Materials PEARLTHANE® 11T85UV Thermoplastic Polyurethane Elastomer
PEARLTHANE® 11T85UV is a UV resistant polycaprolactone copolyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, featuring adequate hardness with excellent..
Injection Pressure 10.0 MPa
1450 psi
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer
PEARLTHANE® CLEAR 15N80 is a polyether copolymer-based TPU, supplied in form of translucent, colorless, combining low hardness with excellent mechanical properties and excellent hydrolysis resist..
Injection Pressure >= 10.0 MPa
>= 1450 psi
Compression and injection cavity mold pressure
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value..
Injection Pressure >= 10.0 MPa
>= 1450 psi
Compression and injection cavity mold pressure
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U..