Polymer Property : Injection Pressure = 2.07 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-001 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-003 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-005 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-026 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-028 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-046 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-050 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-051 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-072 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-081 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-082 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-085 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-089 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-091 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-116 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-214 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-190 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-251 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..