Processing Properties Metric English Comments
Injection Pressure 49.03 - 98.07 MPa
7111 - 14220 psi
LG Chemical KEYFLEX TO-1045D Thermoplastic Olefin for Injection Molding, 45D Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Injection Pressure 49.03 - 98.07 MPa
7111 - 14220 psi
LG Chemical KEYFLEX TO-1075A Thermoplastic Olefin for Injection Molding, 75A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Injection Pressure 49.03 - 98.07 MPa
7111 - 14220 psi
LG Chemical KEYFLEX TO-1088A Thermoplastic Olefin for Injection Molding, 88A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Injection Pressure 49.03 - 98.07 MPa
7111 - 14220 psi
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Injection Pressure 49.03 - 78.45 MPa
7111 - 11380 psi
Second
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Injection Pressure 49.03 - 78.45 MPa
7111 - 11380 psi
Second
LG Chemical LUCON PO-3000 Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Injection Pressure 49.03 - 78.45 MPa
7111 - 11380 psi
Second
LG Chemical LUCON PO-5300H Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Injection Pressure 49.03 - 78.45 MPa
7111 - 11380 psi
Second
LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Injection Pressure 49.03 - 78.45 MPa
7111 - 11380 psi
Second
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Injection Pressure 49.03 - 78.45 MPa
7111 - 11380 psi
First
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Injection Pressure 49.03 - 78.45 MPa
7111 - 11380 psi
Second
LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..