Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE
Manufacturer LG Chemical
Trade Name KEYFLEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber and the strength of engineering plastics. In additions, they offer very good thermal stability, chemical resistance and weather resistance. KEYFLEX resins can be widely accepted as the replacement of thermoset rubbers.Characterization: High impact strengthLow specific gravityExcellent resistance to chemicals and weatheringGood electrical propertiesVarious hardness grades (soft, semi-soft, and hard)ColorabilityRecyclabilityApplications: Automotive: Exterior: Bumper, air spoiler, mud guard, trim, side moldingInterior: Head liner, instrument panel skin, glass sealing, door trim skinOthers: Air intake hose, air duct, lamp packing, weather stripping, handle gasket, boots dustOthers: Hose, packing, phone foots, gasket, insulation sheet (water protection sheet etc.), racket grip, booster cable, pump cableInformation Provided by LG Chem
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 80 - 86
80 - 86
ASTM D2240
Tensile Strength at Break 9.80 MPa
1420 psi
ASTM D412
Tensile Strength, Yield 4.90 MPa

@Strain 100 %
711 psi

@Strain 100 %
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Izod Impact, Notched NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D256
Tear Strength 59.6 kN/m
340 pli
ASTM D790
Processing Properties Metric English Comments
Processing Temperature 160 - 200 °C
320 - 392 °F
Extrusion cylinder temperature
180 - 210 °C
356 - 410 °F
Blow molding cylinder temperature
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Middle Barrel Temperature 200 - 220 °C
392 - 428 °F
Front Barrel Temperature 210 - 230 °C
410 - 446 °F
Nozzle Temperature 210 - 230 °C
410 - 446 °F
Die Temperature 93.3 °C
200 °F
Extrusion
93.3 - 104 °C
200 - 220 °F
Blow molding
Mold Temperature 5.00 - 40.0 °C
41.0 - 104 °F
Blow molding
30.0 - 60.0 °C
86.0 - 140 °F
Injection molding
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 2 hour
2 hour
Hot Blast
Injection Pressure 49.03 - 98.07 MPa
7111 - 14220 psi
Screw Speed 20 - 100 rpm
20 - 100 rpm
Descriptive Properties Value Comments
Ozone Resistance No Crack
ASTM D518