Processing Properties Metric English Comments
Die Opening 0.100 cm
0.0394 in
Cast Film Extrusion
Braskem CX7020 LDPE Cast Film Extrusion Polyethylene
CX7020 is a low-density polyethylene (LDPE) with excellent processability and low gel content. Those features allow for production of thin and highly uniform films. This product is identified as PE ..
Die Opening 0.100 - 0.150 cm
0.0394 - 0.0591 in
Blow Film Extrusion
Braskem TN2005 EVA General Film Copolymer
TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e..
Die Opening 0.100 - 0.150 cm
0.0394 - 0.0591 in
Blow Film Extrusion
Braskem TN2006 EVA General Film Copolymer
TN2006 is an Ethylene-Vinyl Acetate (EVA) copolymer with good mechanical properties, high flexibility and toughness even with low temperature, and excellent optical and heat sealability properties. ..
Die Opening 0.100 cm
0.0394 in
Blow Film Extrusion
Braskem TN2020 EVA General Film Copolymer
TN2020 is an Ethylene-Vinyl Acetate (EVA) copolymer developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Multilayer structures..
Die Opening 0.100 cm
0.0394 in
Blow Film Extrusion
Braskem TN7006 LDPE Blown Film Extrusion Polyethylene
TN7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a great combination of mechanical, optical, and stiffness properties. TN7006 h..
Die Opening 0.100 cm
0.0394 in
Blow Film Extrusion
Braskem TS7003 LDPE Blown Film Extrusion Polyethylene
TS7003 is a low-density polyethylene (LDPE) with high molecular weight that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed. Th..
Die Opening 0.100 cm
0.0394 in
Blow Film Extrusion
Braskem TS7006 LDPE Blown Film Extrusion Polyethylene
TS7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a combination of mechanical, optical, and stiffness properties. TS7006 has a l..
Die Opening 0.100 cm
0.0394 in
Blow Film Extrusion
Braskem TS7010 LDPE Blown Film Extrusion Polyethylene
TS7010 is a low-density polyethylene (LDPE) that presents excellent processability and good mechanical properties. The incorporated additives package warrants a low coefficient of friction (COF) all..
Die Opening 0.100 - 0.150 cm
0.0394 - 0.0591 in
Blow Film Extrusion
Braskem TU3001 LDPE Blown Film Extrusion Polyethylene
TU3001 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties, and good processability. These qualities ensure the production of films with uniform thicknes..
Die Opening 0.100 - 0.150 cm
0.0394 - 0.0591 in
Blow Film Extrusion
Braskem TU3002 LDPE Blown Film Extrusion Polyethylene
TU3002 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties (dart drop and Elmendorf tear strength), and good processability. These qualities ensure the p..
Die Opening 0.100 - 0.150 cm
0.0394 - 0.0591 in
Blow Film Extrusion
Braskem TX7001 LDPE Blown Film Extrusion Polyethylene
TX7001 is a low-density polyethylene (LDPE) with high molecular weight designed to satisfy those applications that require high mechanical strength and environmental stress cracking resistance (ESCR..
Die Opening 0.100 cm
0.0394 in
Blow Film Extrusion
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene
TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness..
Die Opening 0.100 cm
0.0394 in
Blow Film Extrusion
Braskem TX9003 LDPE Blown Film Extrusion Polyethylene
TX9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance, good optical properties, and high stiffness. These characteristics provide, in some applications, down gaug..
Die Opening 0.100 cm
0.0394 in
Blow Film Extrusion
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene
TS9022 is a low-density polyethylene (LDPE) developed specially for automatic overwrap packaging. This resin has a combination of high optical properties and excellent stiffness. The incorporated ad..
Die Opening 0.100 cm
0.0394 in
Blow Film Extrusion
Braskem TS9003 LDPE Blown Film Extrusion Polyethylene
TS9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance along with good optical properties and high stiffness. These characteristics ensure the production of packag..
Die Opening 0.100 cm
0.0394 in
Blow Film Extrusion
Braskem TX7003 LDPE Blown Film Extrusion Polyethylene
TX7003 is a low-density, high molecular-weight polyethylene that offers high mechanical strength. The product's characteristics allow for high versatility and use in various applications due to its ..