Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem TS7010 LDPE Blown Film Extrusion Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem TS7010 LDPE Blown Film Extrusion Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TS7010 is a low-density polyethylene (LDPE) that presents excellent processability and good mechanical properties. The incorporated additives package warrants a low coefficient of friction (COF) allowing better performance in packaging lines. This product is identified as PE 114 according to ASTM D-4976-04a standard specification. It contains antiblocking and slip agent additives. Its applications include films for automatic or semi-automatic packaging of food products (grains, powder or ground products) such as cereals, sugar, salt, and flours.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM-D792
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 350 %
350 %
ASTM-D882
Film Elongation at Break, TD 620 %
620 %
ASTM-D882
Secant Modulus, MD 0.120 GPa
17.4 ksi
2% Secant Modulus; ASTM-D882
Secant Modulus, TD 0.130 GPa
18.9 ksi
2% Secant Modulus; ASTM-D882
Elmendorf Tear Strength MD 310 g
310 g
ASTM-D1922
Elmendorf Tear Strength TD 240 g
240 g
ASTM-D1922
Elmendorf Tear Strength, MD 6.20 g/micron
157 g/mil
ASTM-D1922
Elmendorf Tear Strength, TD 4.80 g/micron
122 g/mil
ASTM-D1922
Dart Drop 3.40 g/micron
86.4 g/mil
ASTM-D1709
Dart Drop Test 170 g
0.375 lb
ASTM-D1709
Film Tensile Strength at Break, MD 23.0 MPa
3340 psi
ASTM-D882
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM-D882
Optical Properties Metric English Comments
Haze 9.5 %
9.5 %
ASTM-D1003
Gloss 58 %
58 %
Angle 45°; ASTM-D2457
85 %
85 %
Angle 60°; ASTM-D2457
Processing Properties Metric English Comments
Die Opening 0.100 cm
0.0394 in
Blow Film Extrusion
Blow-up Ratio (BUR) 2.0 - 3.0
2.0 - 3.0
Blow Film Extrusion
Descriptive Properties Value Comments
Mass Temperature (°C) 175-185
Blow Film Extrusion
Temperature Profile (°C) 155-185
Blow Film Extrusion