Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Head Temperature 185 - 204 °C
365 - 399 °F
Average value: 194 °C Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Head Temperature 185 - 200 °C
365 - 392 °F
Extrusion Molding
Kolon ELLAS K-792A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon.
Head Temperature 185 - 200 °C
365 - 392 °F
Extrusion Molding
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane
ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon.
Head Temperature 185 °C
365 °F
Extrusion Blow Molding
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin
SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa..
Head Temperature 185 °C
365 °F
Borealis Borcell™ HE1123 High Density Polyethylene
Borcell™ HE1123 is a high density polyethylene compound intended for the insulation of radio frequency coaxial cables. Borcell™ HE1123 is designed to give the lowest possible cable attenuation by..
Head Temperature >= 185 °C
>= 365 °F
Borealis Borcell™ LE1120 Low Density Polyethylene for Physically Foamed Cellular Insulation
Borcell LE1120 is a low density polyethylene intended for the insulation of coaxial and radio frequency communication cables.. It contains no additives and is designed to give the lowest possible a..
Head Temperature >= 185 °C
>= 365 °F
Borealis Visico™ ME4425/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation
Visico ME4425/LE4432 is a black, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. ME4425 is a medium-density ethylene vinyl..
Head Temperature >= 185 °C
>= 365 °F
Borealis Visico™ ME4425/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation
Visico ME4425/LE4437 is a natural, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. ME4425 is a medium-density ethylene vin..
Head Temperature 185 °C
365 °F
Equate EFDC-7087 LLDPE Film Extrusion Resin
EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-..
Head Temperature 185 - 190 °C
365 - 374 °F
Equate EMDA-6200 HDPE Blow Molding Resin
EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for ..
Head Temperature 185 - 210 °C
365 - 410 °F
Average value: 196 °C Grade Count:6
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max..