Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 230 - 245 °C | 446 - 473 °F | |
Honeywell Aegis™ PL56HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer
(discontinued **) Description: Aegis PL56HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt v.. |
|||
Head Temperature | 230 - 245 °C | 446 - 473 °F | |
Honeywell Aegis™ PL75HS Medium Viscosity, Heat Stabilized, Flexible Nylon 6
(discontinued **) Description: Aegis PL75HS is a medium viscosity, heat stabilized, flexible nylon 6 especially suited to the production of extrusion profiles offering a combination of good flexibility, toughness and.. |
|||
Head Temperature | 230 - 245 °C | 446 - 473 °F | |
Honeywell Aegis™ PL165HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer
(discontinued **) Description: Aegis PL165HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt .. |
|||
Head Temperature | 230 - 245 °C | 446 - 473 °F | |
Honeywell Aegis™ PL220HS High Viscosity, Heat Stabilized, Flexible Nylon 6
(discontinued **) Description: Aegis PL220HS is a high viscosity, heat stabilized, flexible nylon 6 especially suited to the production of large diameter extrusion or blow molding profiles offering a combination of g.. |
|||
Head Temperature | 235 - 245 °C | 455 - 473 °F | |
Borealis Borcoat™ BB125E Polypropylene Adhesive for Steel Pipe Coating Borcoat BB125E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the top-coat polypropylene Borcoat BB108E-1199.B.. |
|||
Head Temperature | 235 - 245 °C | 455 - 473 °F | |
Borealis Borcoat™ BB127E Polypropylene Adhesive Powder form for Steel Pipe Coating Borcoat BB127E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the Top-coat polypropylene coating Borcoat BB108.. |