Honeywell Aegis™ PL165HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Unreinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell Aegis™ PL165HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Aegis PL165HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt viscosity and optimized crystallization properties, this formulation has been tailored to meet the demanding process behavior requirements of larger diameter extruded profiles. Chemical resistance is excellent to greases, oils and hydrocarbons.Applications:Used in extruded profile applications.Information provided by Honeywell.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Maximum Moisture Content 0.0010
0.0010
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Strength 25.0 MPa
3630 psi
ASTM D790
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 230 - 250 °C
446 - 482 °F
Middle Barrel Temperature 240 - 255 °C
464 - 491 °F
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Die Temperature 230 - 245 °C
446 - 473 °F
Melt Temperature 250 - 260 °C
482 - 500 °F
Head Temperature 230 - 245 °C
446 - 473 °F