Polymer Property : Pot Life = 20160 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life >= 20160 min
>= 20160 min
Resin Technology Group 451 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma..
Pot Life >= 20160 min
>= 20160 min
Resin Technology Group 451 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma..
Pot Life 20160 min
20160 min
Epoxy Technology EPO-TEK® EK1000 Epoxy
Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding ..
Pot Life 20160 min
20160 min
Epoxy Technology EPO-TEK® EK1000-MP Epoxy
Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding ..
Pot Life 20160 min
20160 min
Epoxy Technology EPO-TEK® EK2000 Epoxy
Preliminary Product Information SheetMaterial Description: A two component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance ..
Pot Life 20160 min
20160 min
Epoxy Technology EPO-TEK® M10-D Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..