Polymer Property : Pot Life = 7.00 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 7.00 - 9.00 min
7.00 - 9.00 min
Northstar Polymers MSN-V40A Polyester Base Low-Rebound Impact/Vibration Dampening Gel
This polyurethane casting material is developed for applications that require Shore OO 40 range casting material with vibration dampening property and higher strength than standard polyurethane gel ..
Pot Life 7.00 min

@Temperature 23.9 °C
7.00 min

@Temperature 75.0 °F
3M Scotch-Weld™ 3532 B/A Brown Two-Part Urethane Adhesive 3532 B/A Brown  (discontinued **)
Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 20-30 minutes handling stren..
Pot Life 7.00 - 12.0 min

@Temperature 23.9 °C
7.00 - 12.0 min

@Temperature 75.0 °F
Devcon Combo Wear FC Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.