Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 85.0 °C @Time 10800 sec |
185 °F @Time 3.00 hour |
Horizontal Oven |
Zhejiang Juner JEPP263 Weatherability PP Series Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Drying Temperature | 85.0 °C @Time 10800 sec |
185 °F @Time 3.00 hour |
Horizontal Oven |
Zhejiang Juner JEPPA003 High Glossy PP Applications: High Glossy PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Drying Temperature | 85.0 °C @Time 10800 sec |
185 °F @Time 3.00 hour |
Horizontal Oven |
Zhejiang Juner JEPPB003 High Glossy PP Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Drying Temperature | 85.0 °C @Time 10800 sec |
185 °F @Time 3.00 hour |
Horizontal Oven |
Zhejiang Juner JEPPB005 High Glossy PP Applications: Shell of Air ConditionerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Drying Temperature | 85.0 °C @Time 10800 sec |
185 °F @Time 3.00 hour |
Horizontal Oven |
Zhejiang Juner JEPPB006 High Glossy PP Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Drying Temperature | 85.0 °C @Time 10800 sec |
185 °F @Time 3.00 hour |
Horizontal Oven |
Zhejiang Juner JEPPBC001 Weatherability PP Series Applications: Weatherability ProductsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Drying Temperature | 85.0 °C @Time 10800 sec |
185 °F @Time 3.00 hour |
Horizontal Oven |
Zhejiang Juner PP430R Weatherability PP Series Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |