Polymer Property : Cycle Time - Injection = 1.5 sec Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cycle Time - Injection 1.2 - 1.5 sec
1.2 - 1.5 sec
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r..
Cycle Time - Injection 1.2 - 1.5 sec
1.2 - 1.5 sec
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r..
Cycle Time - Injection 1.2 - 1.5 sec
1.2 - 1.5 sec
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec..