Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 245 - 260 °C | 473 - 500 °F | |
Lavergne VYPET 2130 Polyester Alloy Resin, 30% Fiberglass Reinforced Vypet 2130 is a 30% fiberglass reinforced, toughened Modified PBT injection molding compound designed for structural and electrical applications.Features: High temperature performances; Excellent di.. |
|||
Feed Temperature | 245 - 255 °C | 473 - 491 °F | |
Lavergne VYPET VNT 1020 Polyester-PC Alloy The Vypet 1020 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Feed Temperature | 245 - 255 °C | 473 - 491 °F | |
Lavergne VYPET VNT 1021 Polyester-PC Alloy The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |