Polymer Property : Adapter Temperature = 200 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Adapter Temperature 180 - 200 °C
356 - 392 °F
Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend
The Trilene TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring ..
Adapter Temperature 185 - 200 °C
365 - 392 °F
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film
The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc..
Adapter Temperature 180 - 200 °C
356 - 392 °F
Petroquimica Triunfo Trilene® TS 8058 LLDPE-C6 and LDPE Blend
The Trilene TS 8058 product is a blend with a high ratio of linear low-density polyethylene - hexene comonomer (LLDPE-C6) with low-density polyethylene (LDPE) excellent mechanical resistance, along ..
Adapter Temperature 175 - 200 °C
347 - 392 °F
Extrusion
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester
Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a..
Adapter Temperature 175 - 200 °C
347 - 392 °F
Extrusion
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade
IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially..
Adapter Temperature 175 - 200 °C
347 - 392 °F
Extrusion
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester
Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe..
Adapter Temperature 175 - 200 °C
347 - 392 °F
Extrusion
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether
Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS..
Adapter Temperature 175 - 200 °C
347 - 392 °F
Extrusion
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester
Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par..
Adapter Temperature 180 - 200 °C
356 - 392 °F
Extrusion Molding
LG Chemical KEYFLEX BT 10288D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 180 - 200 °C
356 - 392 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 190 - 200 °C
374 - 392 °F
5
Lubrizol Advanced Materials Pearlthane® D91F88 Thermoplastic Polyurethane Elastomer
Type: Pearlthane® D91F88 is an aliphatic-based thermoplastic polyurethane.Main Application : ExtrusionSpecial features : Outstanding abrasion loss, excellent color stability upon weather exposure..
Adapter Temperature 175 - 200 °C
347 - 392 °F
Extrusion
Huntsman IROGRAN® A 85 P 4854 Ether-Based TPU-For Cable Industry
Introduction: IROGRAN A 85 P 4854 is a flame-retardant, halogen-free polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4854 is part..
Adapter Temperature 190 - 200 °C
374 - 392 °F
Extrusion
Huntsman IROGRAN® A 91 P 4945 TPU-Polyester
Introduction: IROGRAN A 91 P 4945 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 91 P 4945 is part of the HUNTSMAN technical ext..