Adapter Temperature 275 °C
527 °F
For high temperature coextrusions.
DuPont Bynel® 21E553 Adhesive Resin  (discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..
Adapter Temperature 275 °C
527 °F
Arkema Group OREVAC® 18750 Maleic Anhydride Modified Polypropylene
DescriptionOREVAC 18750 is a coextrusion coating adhesive based on a maleic anhydride modified polypropylene resin. It combines the processability of an extrusion coating resin with the thermal resi..
Adapter Temperature 275 °C
527 °F
Arkema Group OREVAC® 18751 Maleic Anhydride Modified Polypropylene
DescriptionOREVAC 18751 is a coextrusion coating adhesive based on a maleic anhydride modified polypropylene resin. It combines the processability of an extrusion coating resin with the thermal resi..