Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Bynel® 21E553 Adhesive Resin  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Bynel® 21E553 Adhesive Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. Applications:Bynel® Series 2100 resins adhere to a wide variety of materials. They are most often used to adhere to PE and PET. They also adhere to EVA, EVOH, polyamide, and PP.Bynel® 21E533 is designed for cast film or extrusion coating processes. The Bynel® Series 2100 resins can be used in a variety of coextrusion coating and laminating applications, e.g., as a tie layer for PET/PE sheet coextrusions replacing rigid PVC.Physical properties of Bynel® Series 2100 resins are typical of polyethylene/acrylate copolymer resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others for a particular extrusion process.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 7.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 64.0 °C
147 °F
Freezing Point, DSC; ASTM D3418
83.0 °C
181 °F
DSC; ASTM D3418
Vicat Softening Point 50.0 °C
122 °F
ASTM D1525
Processing Properties Metric English Comments
Rear Barrel Temperature 120 °C
248 °F
For high temperature coextrusions.
120 °C
248 °F
For film or coating with EVA or EVOH.
Middle Barrel Temperature 220 °C
428 °F
For film or coating with EVA or EVOH.
235 °C
455 °F
For high temperature coextrusions.
Front Barrel Temperature 235 °C
455 °F
For film or coating with EVA or EVOH.
275 °C
527 °F
For high temperature coextrusions.
Adapter Temperature 235 °C
455 °F
For film or coating with EVA or EVOH.
275 °C
527 °F
For high temperature coextrusions.
Die Temperature 235 °C
455 °F
For film or coating with EVA or EVOH.
275 °C
527 °F
For high temperature coextrusions.
Users viewing this material also viewed the following: