Polymer Property : Adapter Temperature = 285 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Adapter Temperature 185 - 285 °C
365 - 545 °F
Average value: 224 °C Grade Count:4
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..