Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 200 - 215 °C | 392 - 419 °F | |
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film.. |
|||
Adapter Temperature | 175 - 215 °C | 347 - 419 °F | Average value: 193 °C Grade Count:43 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Adapter Temperature | 200 - 215 °C | 392 - 419 °F | Extrusion |
Huntsman IROGRAN® A 95 E 4861 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A95 4861 is a high performance polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN A95E 4861 is part of the HUNTSMAN technical extrusion pro.. |