Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 200 °C | 392 °F | |
NatureWorks® Ingeo™ 2003D General Purpose Transparent Extrusion Grade Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed fo.. |
|||
Adapter Temperature | 200 °C | 392 °F | |
NatureWorks® Ingeo™ 4032D Film Grade PLA NatureWorks® PLA (polylactide) polymer 4032D can be converted into a biaxially oriented film with use temperatures up to 300°F (150°C). This film has excellent optics, good machinability and exce.. |
|||
Adapter Temperature | 200 °C | 392 °F | |
NatureWorks® Ingeo™ 4060D Sealant Grade PLA PLA (polylactide) polymer 4060D can be coextruded with other PLA resin to form a sealant layer for biaxially oriented PLA film. This resin has excellent heat seal and hot tack performance with a sea.. |
|||
Adapter Temperature | 200 - 215 °C | 392 - 419 °F | |
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film.. |
|||
Adapter Temperature | 200 - 220 °C | 392 - 428 °F | |
Petroquimica Triunfo Trithene® TU 3001 LDPE - Agricultural Film The Trithene TU 3001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical properties, good processability and bu.. |
|||
Adapter Temperature | 200 - 215 °C | 392 - 419 °F | Extrusion |
Huntsman IROGRAN® A 95 E 4861 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A95 4861 is a high performance polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN A95E 4861 is part of the HUNTSMAN technical extrusion pro.. |
|||
Adapter Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information .. |
|||
Adapter Temperature | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1140D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3028D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical LG713 ABS, Low Gloss Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical MU620 ABS, Low Deformation Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical SH610S ABS, Excellent Surface, High Impact Feature: Extrusion Molding, Excellent Surface, High ImpactApplication: Bag, miscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical SH625 ABS, High Impact, High Flow Feature: Extrusion Molding, High Impact, High FlowApplication: Ski Flat, MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Adapter Temperature | 200 - 230 °C | 392 - 446 °F | 5 |
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mec.. |
|||
Adapter Temperature | 200 - 220 °C | 392 - 428 °F | 5 |
Lubrizol Advanced Materials PEARLTHANE® 11T85E Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11T85E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
Adapter Temperature | 200 °C | 392 °F | |
Taiwan PU Corporation TPUI-E95 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Adapter Temperature | 200 °C | 392 °F | |
Taiwan PU Corporation TPUI-H95 High Hydrolysis Resistance, Injection Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Adapter Temperature | 200 °C | 392 °F | |
Taiwan PU Corporation TPUI-L90 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Adapter Temperature | 200 °C | 392 °F | |
SK Chemicals SKYTHANE® S195A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Adapter Temperature | 200 °C | 392 °F | |
SK Chemicals SKYTHANE® S198A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Adapter Temperature | 200 °C | 392 °F | |
SK Chemicals SKYTHANE® S395A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Adapter Temperature | 200 °C | 392 °F | |
SK Chemicals SKYTHANE® X595A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Adapter Temperature | 200 °C | 392 °F | |
SK Chemicals SKYTHANE® R195A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Adapter Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |