Processing Properties Metric English Comments
Adapter Temperature 200 - 220 °C
392 - 428 °F
Petroquimica Triunfo Trithene® TU 3001 LDPE - Agricultural Film
The Trithene TU 3001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical properties, good processability and bu..
Adapter Temperature 200 - 220 °C
392 - 428 °F
Petroquimica Triunfo Trithene® TU 8091 LDPE - Agricultural Film
Trithene TU 8091 is a low-density polyethylene (LDPE) with high molecular weight, with excellent mechanical properties and good processability. These qualities ensure the production of very wide fil..
Adapter Temperature 200 - 220 °C
392 - 428 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1033D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 200 - 220 °C
392 - 428 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1040D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 200 - 220 °C
392 - 428 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1045D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 200 - 220 °C
392 - 428 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1140D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 200 - 220 °C
392 - 428 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3028D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 200 - 220 °C
392 - 428 °F
5
Lubrizol Advanced Materials PEARLTHANE® 11T85E Thermoplastic Polyurethane Elastomer
Type: Pearlthane® 11T85E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr..
Adapter Temperature 200 - 220 °C
392 - 428 °F
5
Lubrizol Advanced Materials PEARLTHANE® 11T92E Thermoplastic Polyurethane Elastomer
Type: Pearlthane® 11T92E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr..