Die Temperature 154 °C
309 °F
Extrusion
Huntsman IROGRAN® CA116-203 TPU-Polyester
Introduction: IROGRAN CA116-203 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-203 is part of the HUNTSMAN film and shee..
Die Temperature 154 °C
309 °F
Extrusion
Huntsman IROGRAN® CA116-205 TPU-Polyester
Introduction: IROGRAN CA116-205 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-205 is part of the HUNTSMAN film and shee..