Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | >= 168 °C | >= 335 °F | |
Borealis Casico™ FR4804 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing Borstar FR4804 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4804 offers a unique combination of good extrusion p.. |
|||
Die Temperature | 168 - 182 °C | 335 - 360 °F | |
Axiall 3014 Rigid PVC, Extrusion Georgia Gulf 3014 is a base for use of wood flour up to 40 percent. Impact Strength & ToughnessFlame RetardantChemical ResistanceDimensional StabilityInformation provided by Georgia GulfGeorgia Gul.. |
|||
Die Temperature | 168 - 182 °C | 335 - 360 °F | |
Axiall 3020 Rigid PVC, Extrusion Georgia Gulf 3020 is a base for use of wood flour up to 40 percent. Impact strength and toughnessFlame retardantChemical resistanceDimensional stabilityInformation provided by Georgia GulfGeorgia G.. |