Processing Properties Metric English Comments
Die Temperature 191 - 224 °C
375 - 435 °F
Extrusion
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Die Temperature 196 - 224 °C
385 - 435 °F
Extrusion
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer
A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..