Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 220 - 250 °C | 428 - 482 °F | Average value: 238 °C Grade Count:6 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Die Temperature | 220 - 250 °C | 428 - 482 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1155D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Extrusion Molding |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Extrusion Molding |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical MU620 ABS, Low Deformation Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical SH625 ABS, High Impact, High Flow Feature: Extrusion Molding, High Impact, High FlowApplication: Ski Flat, MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Pipe Extrusion |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Tube Extrusion |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Tube Extrusion |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Die Temperature | 220 - 250 °C | 428 - 482 °F | Extrusion Molding |
LG Chemical KEYFLEX BT S5035 Ester Type TPE Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide.. |
|||
Die Temperature | 220 - 250 °C | 428 - 482 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Die Temperature | 210 - 250 °C | 410 - 482 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |