Processing Properties Metric English Comments
Die Temperature 200 - 250 °C
392 - 482 °F
Extrusion Molding
LG Chemical LI931 Extrusion ASA
Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical
Die Temperature 200 - 250 °C
392 - 482 °F
Extrusion Molding
LG Chemical MU620 ABS, Low Deformation
Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical
Die Temperature 200 - 250 °C
392 - 482 °F
Extrusion Molding
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Die Temperature 200 - 250 °C
392 - 482 °F
Extrusion Molding
LG Chemical SH610A ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical
Die Temperature 210 - 250 °C
410 - 482 °F
Ineos ABS Lustran® Guardian™ 620 ABS, Extrusion Grade
Lustran® Guardian™ ABS 620 is a high modulus, HFC 134a and HCFC 22 resistant extrusion grade resin designed for refrigerator door and food liners. Lustran® ABS 620 offers good melt streng..
Die Temperature 240 - 250 °C
464 - 482 °F
Arkema Group OREVAC® 18319 Grafted Maleic Anhydride Polyethylene
OREVAC 18319 is a maleic anhydride grafted polyethylene used in the manufacturing of multi-layer aluminium panels. OREVAC 18319 is mainly used in aluminium panels to have good adhesion performances ..
Die Temperature 210 - 250 °C
410 - 482 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Die Temperature 210 - 250 °C
410 - 482 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Die Temperature 210 - 250 °C
410 - 482 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Die Temperature 210 - 250 °C
410 - 482 °F
Tube Extrusion
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Die Temperature 210 - 250 °C
410 - 482 °F
Tube Extrusion
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Die Temperature 210 - 250 °C
410 - 482 °F
Tube Extrusion
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Die Temperature 210 - 250 °C
410 - 482 °F
Tube Extrusion
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Die Temperature 210 - 250 °C
410 - 482 °F
Tube Extrusion
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Die Temperature 220 - 250 °C
428 - 482 °F
Extrusion Molding
LG Chemical KEYFLEX BT S5035 Ester Type TPE
Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide..
Die Temperature 220 - 250 °C
428 - 482 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Die Temperature 210 - 250 °C
410 - 482 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Die Temperature 210 - 250 °C
410 - 482 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..