Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 204 °C | 400 °F | Compression Zone |
Lubrizol Advanced Materials PEARLTHANE® 16N87 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® D16N87 is a polyether-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, offering adequate hardness with superior hydrolysis resistance and improved e.. |
|||
Zone 1 | 204 °C | 400 °F | Compression Zone |
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b.. |
|||
Zone 1 | 204 °C | 399 °F | Extrusion |
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 70DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig.. |
|||
Zone 1 | 204 °C | 399 °F | Extrusion |
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig.. |
|||
Zone 1 | 204 °C | 399 °F | |
Equate EMDA-6147 HDPE Blow Molding Resin EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density.. |