Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66 Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66 Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66 Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66 Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc.. |
|||
Zone 1 | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 1700-7859 PPO, with carbon fiber, glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Improved friction and wear behaviour... |
|||
Zone 1 | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 1700-7910 PPO, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Zone 1 | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 1700-8541 PPO, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Isotropic shrinkage characteristics.Superheated steam sterilizable.Infor.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Starflam RF0069 PA66, 30% Glass Fiber, Flame Retardant, Injection Molded Starflam RF0069 is a Flame Retardant, 30% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as PA66 30V U2 Z79 or RF1006Z590)Information provided by Eurostar. |
|||
Zone 1 | 270 - 280 °C | 518 - 536 °F | |
Eurostar Starflam RF023P PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0023P is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding (also known as Starflam PA66C U2 Z23)Information provided by Eurostar. |
|||
Zone 1 | 270 °C | 518 °F | Feed Zone |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Zone 1 | 270 °C | 518 °F | Feed Zone |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Zone 1 | 270 °C | 518 °F | Feed Zone |
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry) Description: Ultramid® BG40GM45 HS BK-130 is a pigmented black, heat stabilized, 45 % glass and mineral fiber reinforced polyamide 6 injection molding compound. It possesses a balance of engineerin.. |
|||
Zone 1 | 270 - 280 °C | 518 - 536 °F | |
Lehmann & Voss LUVOCOM® 1700-7903 PPO, with glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r.. |