Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1700-7903 PPO, with glass fiber, lubricant modified

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, 10% Glass Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1700-7903 PPO, with glass fiber, lubricant modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance range.Especially suitable for thin wall complex parts.Emergency running property.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 22.32 g/10 min

@Load 5.00 kg,
Temperature 300 °C
22.32 g/10 min

@Load 11.0 lb,
Temperature 572 °F
Mechanical Properties Metric English Comments
Tensile Stress 80.0 MPa
11600 psi
Elongation at Yield 2.5 %
2.5 %
3.2 %
3.2 %
flexural
Modulus of Elasticity 4.50 GPa
653 ksi
Flexural Strength 105 MPa
15200 psi
Flexural Modulus 4.00 GPa
580 ksi
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
flatwise; ISO 179 1fU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
130 °C
266 °F
short term
Flammability, UL94 HB
HB
not recognized by UL
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 280 °C
536 °F
mass temp
Nozzle Temperature 285 - 295 °C
545 - 563 °F
Zone 1 270 - 280 °C
518 - 536 °F
Zone 2 270 - 300 °C
518 - 572 °F
Zone 3 290 - 305 °C
554 - 581 °F
Mold Temperature 70.0 - 120 °C
158 - 248 °F
Drying Temperature 95.0 - 110 °C

@Time <=7200 sec
203 - 230 °F

@Time <=2.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (white)