Processing Properties Metric English Comments
Zone 2 179 °C
354 °F
Extrusion
Lubrizol ESTANE® 58284 Ether Based Thermoplastic Polyurethane
Features: Matte finish, superior durabilityUses: Extrusion – wire and cable, General applicationAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Zone 2 179 °C
354 °F
Extrusion
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti..