Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 190 °C | 374 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 5300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5300 is a static dissipative thermoplastic compound based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance valu.. |
|||
Zone 2 | 190 °C | 374 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Zone 2 | 190 °C | 374 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be.. |
|||
Zone 2 | 190 - 210 °C | 374 - 410 °F | Blow Molding |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Zone 2 | 190 - 210 °C | 374 - 410 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1047D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical LG713 ABS, Low Gloss Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Zone 2 | 190 - 210 °C | 374 - 410 °F | Extrusion Molding |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 2 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical SH625 ABS, High Impact, High Flow Feature: Extrusion Molding, High Impact, High FlowApplication: Ski Flat, MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Zone 2 | 190 °C | 374 °F | |
SK Chemicals SKYTHANE® S198A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 2 | 190 °C | 374 °F | |
SK Chemicals SKYTHANE® S398A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Zone 2 | 190 - 200 °C | 374 - 392 °F | Injection |
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol. |
|||
Zone 2 | 190 - 200 °C | 374 - 392 °F | Injection |
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 2 | 190 °C | 374 °F | Extrusion Coating |
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a .. |
|||
Zone 2 | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starflam M10004A PP, Flame Retardant, Injection Molding Starflam M10004A is an Unfilled Halogen Free Flame Retardant PP injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding Starflam MX05036 is an Unfilled, Halogen Free Flame Retardant, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 2 | 190 °C | 374 °F | Extrusion |
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 2 | 190 °C | 374 °F | Extrusion |
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 2 | 190 °C | 374 °F | Extrusion |
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Zone 2 | 190 °C | 374 °F | Extrusion |
Alliance Polymers Viprene™ P85A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |