Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Eurostar Engineering Plastics
Trade Name Starflam
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Starflam MX05036 is an Unfilled, Halogen Free Flame Retardant, Polypropylene Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.013 - 0.015 cm/cm

@Time 86400 sec
0.013 - 0.015 in/in

@Time 24.0 hour
E2P method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527
Elongation at Break >= 500 %
>= 500 %
ISO 527
Flexural Strength 28.0 MPa
4060 psi
ISO 178
Flexural Modulus 1.30 GPa
189 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Processing Properties Metric English Comments
Zone 1 180 - 190 °C
356 - 374 °F
Zone 2 190 - 200 °C
374 - 392 °F
Zone 3 190 - 200 °C
374 - 392 °F
Melt Temperature 190 - 200 °C
374 - 392 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Drying Temperature 70.0 °C

@Time 10800 sec
158 °F

@Time 3.00 hour
Copyright © lookpolymers.com All Rights Reserved