Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 170 - 220 °C | 338 - 428 °F | |
Lehmann & Voss LUVOCOM® 94-8485 LD-PE, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable .. |
|||
Zone 2 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 2 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3028D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 2 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT GN7142F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Low ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Zone 2 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical LI933 Co-Extrusion ASA Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical |
|||
Zone 2 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Zone 2 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Zone 2 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | |
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance.. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | |
Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding application.. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | Extrusion |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | Injection |
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | Injection |
Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr.. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | Injection |
Lubrizol ESTANE® GP65DE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | Injection |
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati.. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | Injection |
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | |
Eurostar Starglas FF001 HDPE, Glass Fiber Filled Starglas FF001 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | |
Eurostar Starglas FF004 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | |
Eurostar Starglas FX05032 PE Starglas FX05032 is Polyethylene Resin with a Proprietary Additive (foaming agent for polyolefins)Information provided by Eurostar. |
|||
Zone 2 | 195 - 220 °C | 383 - 428 °F | |
Arkema Group OREVAC® 18760 Grafted Maleic Anhydride Polypropylene OREVAC 18760 is a maleic anhydride grafted polypropylene used in the manufacturing of three layer PP coating for steel pipeline. OREVAC 18760 is also used in multilayer EVOH – PP structures. OREVAC.. |
|||
Zone 2 | 200 - 220 °C | 392 - 428 °F | Extrusion Molding |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |