Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 210 °C | 410 °F | Die |
Premix Thermoplastics PRE-ELEC® ESD 5350 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5350 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Zone 2 | 210 °C | 410 °F | Die |
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Zone 2 | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical KEYFLEX BT GN7155F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Zone 2 | 210 - 230 °C | 410 - 446 °F | Extrusion |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Zone 2 | 210 - 230 °C | 410 - 446 °F | Extrusion |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | |
Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding application.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Nitric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 - 220 °C | 410 - 428 °F | Injection |
Lubrizol Estane® GP 58 DT Thermoplastic Polyurethane Type: Estane® GP 58DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding parts, animal identification tagsAvailable in E.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C/E10 for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C/E10 for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 °C | 410 °F | Extrusion Coating |
DuPont™ Appeel® 20D855 Ethylene Acrylate DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Zone 2 | 210 °C | 410 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Zone 2 | 210 °C | 410 °F | |
AdvanSource Biomaterials ChronoFlex® AL 65D Biodurable Medical Grade Polyurethane ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3035JX47 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: conductiveInformation provided by UBE. |
|||
Zone 2 | 210 °C | 410 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® 1706 Zinc Ionomer Surlyn® 1706 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |
|||
Zone 2 | 210 °C | 410 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® 2601B Sodium Ionomer Surlyn® 2601B is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer .. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Xylene for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 210 °C | 410 °F | For T-Die Cast Film Extrusion |
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |