Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 149 - 193 °C | 300 - 379 °F | |
Styrolution PS-168M Polystyrene Description: Polystyrene 168M is a high heat, high molecular weight general purpose polystyrene with excellent clarity and high stiffness. Due to its high melt strength and high stiffness. PS-168M i.. |
|||
Zone 2 | 177 - 193 °C | 351 - 379 °F | |
Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Zone 2 | 183 - 193 °C | 361 - 379 °F | Extrusion |
Lubrizol Estane® 58280 Thermoplastic Polyurethane Type: Estane® 58280 is a polyether-type thermoplastic polyurethane (TPU) compound.Features: High resiliency compound, with unique physical properties such as low tensile and compression set, high r.. |