Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
Melt Flow 0.75 g/10 min
0.75 g/10 min
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
Tensile Strength at Break 15.2 MPa
2200 psi
Tensile Strength, Yield 11.7 MPa
1700 psi
Elongation at Break 650 %
650 %
1% Secant Modulus 345 MPa
50000 psi
Thermal Properties Metric English Comments
Brittleness Temperature <= -76.0 °C
<= -105 °F
Electrical Properties Metric English Comments
Dielectric Constant 2.29
2.29
Dissipation Factor 0.000060
0.000060
Processing Properties Metric English Comments
Feed Temperature 154 - 163 °C
309 - 325 °F
Zone 2 177 - 193 °C
351 - 379 °F
Zone 3 193 - 210 °C
379 - 410 °F
Zone 4-x 204 - 218 °C
399 - 424 °F
Adapter Temperature 204 - 218 °C
399 - 424 °F
Die Temperature 204 - 218 °C
399 - 424 °F
Copyright © lookpolymers.com All Rights Reserved